Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Secant Modulus | 10.8 GPa @Strain 1.15 %, Temperature 23.0 °C |
1570 ksi @Strain 1.15 %, Temperature 73.4 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Rynite® 540SUV BK544 Polyethylene Terephthalate (PET)
(Unverified Data**) 40% Glass Reinforced UV Stabilized Polyethylene Terephthalate Developed for Extrusion and Injection Molding Rynite 540SUV BK544 is a 40% glass fiber reinforced UV stabilized modified polyethylene te.. |
|||
Secant Modulus | 10.8 GPa @Strain 0.110 %, Temperature 23.0 °C |
1570 ksi @Strain 0.110 %, Temperature 73.4 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Rynite® 935SUV BK593 Polyethylene Terephthalate (PET)
(Unverified Data**) 35% Glass Reinforced UV Stabilized Polyethylene Terephthalate Rynite 935SUV BK593 is a 35% glass fiber /mineral reinforced UV stabilized modified polyethylene terephthalate resin with low warpage de.. |
|||
Secant Modulus | 10.8 GPa @Strain 1.40 %, Temperature -40.0 °C |
1560 ksi @Strain 1.40 %, Temperature -40.0 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Rynite® FR530 NC010 Polyethylene Terephthalate (PET)
(Unverified Data**) 30% Glass Reinforced Flame Retardant Polyethylene Terephthalate Rynite FR530 NC010 is a 30% glass reinforced flame retardant modified polyethylene terephthalate resin.Information provided by DuPont .. |
|||
Secant Modulus | 10.8 GPa @Strain 0.510 %, Temperature 23.0 °C |
1560 ksi @Strain 0.510 %, Temperature 73.4 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Rynite® RE5329 BK503 Polyethylene Terephthalate (PET)
(Unverified Data**) 36% Glass Reinforced Polyethylene TerephthalateInformation provided by DuPont Performance Polymers |
|||
Secant Modulus | 10.8 GPa @Strain 0.450 %, Temperature 23.0 °C |
1570 ksi @Strain 0.450 %, Temperature 73.4 °F |
DAM; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® EFE7374 BK416 Nylon 6
(Unverified Data**) 40% Glass Reinforced Toughened Polyamide 6 Zytel EFE7374 is a 40% fiber reinforced heat stabilized lubricated toughened polyamide 6 for injection molding. It has an improved impact resistance and ex.. |