Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Secant Modulus | 1.67 GPa @Strain 4.30 %, Temperature 0.000 °C |
242 ksi @Strain 4.30 %, Temperature 32.0 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Delrin® 500TL NC010 Acetal (POM)
(Unverified Data**) Teflon® Lubricated Medium Viscosity Acetal Homopolymer with Low Wear and Low Friction Delrin 500TL is a medium viscosity acetal homopolymer resin containing 1.5% Teflon PTFE Micropowder. It is desi.. |
|||
Secant Modulus | 1.67 GPa @Strain 4.40 %, Temperature 0.000 °C |
242 ksi @Strain 4.40 %, Temperature 32.0 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Delrin® 511DP NC010 Acetal (POM)
(Unverified Data**) Nucleated Medium Viscosity Acetal Homopolymer Delrin 511DP is a medium viscosity acetal homopolymer with improved thermal stability and modifications for more precise molding (reduced warpage less s.. |
|||
Secant Modulus | 1.67 GPa @Strain 4.50 %, Temperature -20.0 °C |
242 ksi @Strain 4.50 %, Temperature -4.00 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Delrin® FG500P NC010 Acetal (POM)
(Unverified Data**) Medium Viscosity Acetal Homopolymer Developed for Food Contact Applications Delrin FG500P is a medium viscosity acetal homopolymer with improved thermal stability. It has been developed for consider.. |
|||
Secant Modulus | 1.67 GPa @Strain 4.30 %, Temperature 0.000 °C |
242 ksi @Strain 4.30 %, Temperature 32.0 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Delrin® FG500TL NC010 Acetal (POM)
(Unverified Data**) Teflon® Lubricated Medium Viscosity Acetal Homopolymer with Low Wear and Low Friction Developed for Food Contact ApplicationsDelrin FG500TL medium viscosity acetal homopolymer resin containing 1.5%.. |
|||
Secant Modulus | 1.67 GPa @Strain 4.40 %, Temperature 0.000 °C |
242 ksi @Strain 4.40 %, Temperature 32.0 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Delrin® FG511DP NC010 Acetal (POM)
(Unverified Data**) Nucleated Medium Viscosity Acetal Homopolymer Developed for Food Contact Applications Delrin FG511DP is a medium viscosity acetal homopolymer with improved thermal stability and modifications for mo.. |
|||
Secant Modulus | 1.67 GPa @Strain 4.84 %, Temperature -20.0 °C |
242 ksi @Strain 4.84 %, Temperature -4.00 °F |
DAM; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® RS LC3090 NC010 Nylon 610
(Unverified Data**) Unreinforced Renewably Sourced High Viscosity Polyamide 610 Developed for Extrusion Zytel RS LC3090 NC010 is a renewable sourced polyamide 610 containing a miniumu of 60% renewably sourced ingredien.. |
|||
Secant Modulus | 1.67 GPa @Strain 2.40 %, Temperature 100 °C |
243 ksi @Strain 2.40 %, Temperature 212 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Sorona® 3015G NC010 Polytrimethylene Terephthalate (PTT)
(Unverified Data**)& 15% Glass Reinforced Polytrimethylene Terephthalate with Resin Made from Bio-PDO Sorona 3015G NC010 is a 15% glass reinforced PTT resin containing 31% renewably sourced ingredients by weight (37% ba.. |