Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Secant Modulus | 1.63 GPa @Strain 5.01 %, Temperature -20.0 °C |
237 ksi @Strain 5.01 %, Temperature -4.00 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Delrin® 300CP NC010 Acetal (POM)
(Unverified Data**) Medium-high Viscosity Acetal Homopolymer with Improved ProcessingDelrin 300CP is a medium-high viscosity acetal homopolymer with improved thermal stability and an outstanding balance of ease of proc.. |
|||
Secant Modulus | 1.63 GPa @Strain 5.86 %, Temperature -40.0 °C |
237 ksi @Strain 5.86 %, Temperature -40.0 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Delrin® 311DP NC010 Acetal (POM)
(Unverified Data**) Nucleated Medium-high Viscosity Acetal Homopolymer Delrin 311DP is a medium-high viscosity acetal homopolymer with enhanced crystallization and balance of part performance and ease of processing. It.. |
|||
Secant Modulus | 1.63 GPa @Strain 4.20 %, Temperature -40.0 °C |
237 ksi @Strain 4.20 %, Temperature -40.0 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Delrin® 520MP NC010 Acetal (POM)
(Unverified Data**) 20% Teflon® Lubricated Medium Viscosity Acetal Homopolymer with Low Wear and Low Friction Delrin 520MP is a medium viscosity acetal homopolymer containing 20% Teflon PTFE Micropowder. It is designe.. |
|||
Secant Modulus | 1.63 GPa @Strain 5.86 %, Temperature -40.0 °C |
237 ksi @Strain 5.86 %, Temperature -40.0 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Delrin® FG311DP NC010 Acetal (POM)
(Unverified Data**) Nucleated Medium-high Viscosity Acetal Homopolymer Developed for Food Contact Applications Delrin FG311DP is a medium-high viscosity acetal homopolymer with improved thermal stability and modificati.. |
|||
Secant Modulus | 1.63 GPa @Strain 3.00 %, Temperature 0.000 °C |
236 ksi @Strain 3.00 %, Temperature 32.0 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Crastin® ST830FRUV NC010 Polybutylene Terephthalate (PBT)
(Unverified Data**) Unreinforced Flame Retardant UV Stabilized Polybutylene Terephthalate Crastin ST830FRUV NC010 is an unreinforced Super Tough flame retardant polybutylene terephthalate resin for injection molding. I.. |
|||
Secant Modulus | 1.63 GPa @Strain 3.20 %, Temperature 80.0 °C |
237 ksi @Strain 3.20 %, Temperature 176 °F |
DAM; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® 70G13HS1L NC010 Nylon 66
(Unverified Data**) 13% Glass Reinforced Heat Stabilized Polyamide 66 Zytel 70G13HS1L NC010 is a 13% glass fiber reinforced heat stabilized polyamide 66 resin for injection molding.Information provided by DuPont Perfor.. |