Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Secant Modulus | 1.05 GPa @Strain 2.10 %, Temperature 40.0 °C |
152 ksi @Strain 2.10 %, Temperature 104 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Crastin® S600F20 NC010 Polybutylene Terephthalate (PBT)
(Unverified Data**)&l Unreinforced Medium Viscosity Polybutylene Terephthalate Crastin S600F20 NC010 is an unreinforced lubricated medium viscosity polybutylene terephthalate resin for injection molding.Information provi.. |
|||
Secant Modulus | 1.05 GPa @Strain 2.10 %, Temperature 40.0 °C |
152 ksi @Strain 2.10 %, Temperature 104 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Crastin® S600F20UV WT660 Polybutylene Terephthalate (PBT) Unreinforced UV Stabilized Polybutylene Terephthalate Crastin S600F20 NC010 is an unreinforced lubricated medium viscosity polybutylene terephthalate resin for injection molding.Information provided.. |
|||
Secant Modulus | 1.05 GPa @Strain 1.20 %, Temperature 80.0 °C |
152 ksi @Strain 1.20 %, Temperature 176 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Delrin® 127UV NC010 Acetal (POM)
(Unverified Data**) UV Stabilized High Viscosity Acetal HomopolymerDelrin 127UV is a high viscosity acetal homopolymer with UV stabilizers developed for automotive interior applications. It has improvements in UV aging.. |
|||
Secant Modulus | 1.05 GPa @Strain 3.50 %, Temperature 100 °C |
152 ksi @Strain 3.50 %, Temperature 212 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Crastin® SK641FR NC010 Polybutylene Terephthalate (PBT) 10% Glass Reinforced Flame Retardant Polybutylene Terephthalate Information provided by DuPont Performance Polymers |
|||
Secant Modulus | 1.05 GPa @Strain 2.40 %, Temperature 40.0 °C |
153 ksi @Strain 2.40 %, Temperature 104 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Crastin® ST830FRUV NC010 Polybutylene Terephthalate (PBT)
(Unverified Data**) Unreinforced Flame Retardant UV Stabilized Polybutylene Terephthalate Crastin ST830FRUV NC010 is an unreinforced Super Tough flame retardant polybutylene terephthalate resin for injection molding. I.. |