Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Secant Modulus | 1.01 GPa @Strain 7.00 %, Temperature 23.0 °C |
146 ksi @Strain 7.00 %, Temperature 73.4 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Delrin® 900P NC010 Acetal (POM)
(Unverified Data**) Low Viscosity Acetal Homopolymer with Improved Processing Delrin 900P is a low viscosity acetal homopolymer for injection molding. It has improved processing thermal stability good mechanical proper.. |
|||
Secant Modulus | 1.01 GPa @Strain 7.00 %, Temperature 23.0 °C |
146 ksi @Strain 7.00 %, Temperature 73.4 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Delrin® FG900P NC010 Acetal (POM)
(Unverified Data**) Low Viscosity Acetal Homopolymer Developed for Food Contact Applications Delrin FG900P is a low viscosity acetal homopolymer with improved thermal stability. It has been developed for consideration .. |
|||
Secant Modulus | 1.01 GPa @Strain 5.47 %, Temperature 200 °C |
147 ksi @Strain 5.47 %, Temperature 392 °F |
DAM; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® HTN 51G35EF BK083 Polyphthalamide (PPA)
(Unverified Data**) 35% Glass Reinforced PPA High Performance Polyamide Developed for Electrical and Electronics Applications Zytel HTN51G35EF BK083 is a 35% glass reinforced heat stabilized lubricated high performance.. |
|||
Secant Modulus | 1.01 GPa @Strain 5.47 %, Temperature 200 °C |
147 ksi @Strain 5.47 %, Temperature 392 °F |
DAM; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® HTN 51G35HSL BK083 Polyphthalamide (PPA)
(Unverified Data**) 35% Glass Reinforced PPA High Performance Polyamide Zytel HTN51G35HSL BK083 is a 35% glass reinforced heat stabilized lubricated high performance polyamide resin. It is also a PPA resin.Information .. |