Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Secant Modulus | 0.832 GPa @Strain 8.80 %, Temperature 0.000 °C |
121 ksi @Strain 8.80 %, Temperature 32.0 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Delrin® 127UV NC010 Acetal (POM)
(Unverified Data**) UV Stabilized High Viscosity Acetal HomopolymerDelrin 127UV is a high viscosity acetal homopolymer with UV stabilizers developed for automotive interior applications. It has improvements in UV aging.. |