Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Secant Modulus | 0.744 GPa @Strain 8.78 %, Temperature 0.000 °C |
108 ksi @Strain 8.78 %, Temperature 32.0 °F |
50%RH; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® RS LC3090 NC010 Nylon 610
(Unverified Data**) Unreinforced Renewably Sourced High Viscosity Polyamide 610 Developed for Extrusion Zytel RS LC3090 NC010 is a renewable sourced polyamide 610 containing a miniumu of 60% renewably sourced ingredien.. |
|||
Secant Modulus | 0.744 GPa @Strain 13.0 %, Temperature -40.0 °C |
108 ksi @Strain 13.0 %, Temperature -40.0 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Delrin® 100 BK602 Acetal (POM)
(Unverified Data**) High Viscosity Acetal Homopolymer Delrin 100 is a high viscosity acetal homopolymer for use in easy to fill molds. Delrin 100 provides maximum toughness in the product line without modification and .. |