Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Secant Modulus | 0.408 GPa @Strain 20.8 %, Temperature -20.0 °C |
59.2 ksi @Strain 20.8 %, Temperature -4.00 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Delrin® 127UV NC010 Acetal (POM)
(Unverified Data**) UV Stabilized High Viscosity Acetal HomopolymerDelrin 127UV is a high viscosity acetal homopolymer with UV stabilizers developed for automotive interior applications. It has improvements in UV aging.. |