Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Secant Modulus | 0.294 GPa @Strain 11.02 %, Temperature 40.0 °C |
42.6 ksi @Strain 11.02 %, Temperature 104 °F |
50%RH; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® RS LC3090 NC010 Nylon 610
(Unverified Data**) Unreinforced Renewably Sourced High Viscosity Polyamide 610 Developed for Extrusion Zytel RS LC3090 NC010 is a renewable sourced polyamide 610 containing a miniumu of 60% renewably sourced ingredien.. |