Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Secant Modulus | 0.198 GPa @Strain 24.2 %, Temperature 0.000 °C |
28.6 ksi @Strain 24.2 %, Temperature 32.0 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Delrin® 100ST NC010 Acetal (POM)
(Unverified Data**) Super Toughened High Viscosity Acetal Homopolymer Delrin 100ST NC010 is a super tough high viscosity acetal homopolymer grade with superior impact resistance. It is designed for highly stressed part.. |
|||
Secant Modulus | 0.198 GPa @Strain 4.87 %, Temperature 100 °C |
28.8 ksi @Strain 4.87 %, Temperature 212 °F |
50%RH; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® RS 3261TL NC010 Nylon 610
(Unverified Data**) Toughened Renewably Sourced Polyamide 610 Developed for Injection Molding Zytel RS 3261TL NC010 is a renewably sourced polyamide 610 resin containing a minimum of 47% renewably sourced ingredient by.. |