Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Secant Modulus | 0.0531 GPa @Strain 33.11 %, Temperature 100 °C |
7.70 ksi @Strain 33.11 %, Temperature 212 °F |
DAM; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® RS 3261TL NC010 Nylon 610
(Unverified Data**) Toughened Renewably Sourced Polyamide 610 Developed for Injection Molding Zytel RS 3261TL NC010 is a renewably sourced polyamide 610 resin containing a minimum of 47% renewably sourced ingredient by.. |