Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Modulus | 0.0172 - 33.8 GPa | 2.49 - 4900 ksi | Average value: 12.2 GPa Grade Count:7 |
Overview of materials for Vinyl Ester Sheet Molding Compound This property data is a summary of similar materials in the MatWeb database for the category "Vinyl Ester Sheet Molding Compound". Each property range of values reported is minimum and maximum value.. |