Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Modulus | 60.0 GPa | 8700 ksi | Compression Warp, Dry/RT; Pr EN 2856 TA |
Hexcel® HexFlow® RTM 6 180°C Epoxy System for Resin Transfer Molding Monocomponent System HexFlow® RTM 6 is a monocomponent resin already degassed, specifically developed to fulfill the requirements of the aerospace and space industries in advanced resin transfer moulding (RTM) process... |
|||
Compressive Modulus | 60.0 GPa @Temperature 75.0 °C |
8700 ksi @Temperature 167 °F |
90º, Wet; DIN65380 |
Hexcel® HexPly® M12 135°C Curing Epoxy Matrix, 45% 46280 Fiber Information provided by HexCel |