Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Modulus | 57.0 GPa @Temperature 175 °C |
8270 ksi @Temperature 347 °F |
Material as cured |
Hexcel® HexPly® 922-1/35%/G926 180°C Curing Epoxy Matrix 5H satin/370g/m2 carbon fabric: FVC=60%Information provided by HexCel |
|||
Compressive Modulus | 57.0 GPa | 8270 ksi | RT; Dry; DIN65380 |
Hexcel® HexPly® M12 135°C Curing Epoxy Matrix, 45% 46280 Fiber Information provided by HexCel |