Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Modulus | 2.34 GPa | 339 ksi | |
Trelleborg AEM Syntac® 350 Syntactic Foam Syntac® 350 is made from high grade epoxy resin and hollow glass microspheres designed specifically for fabricating thermoforming plugs and other associated tooling.Available in block, sheet and ro.. |
|||
Compressive Modulus | 2.34 GPa | 339 ksi | |
Trelleborg AEM Syntac® 351 Syntactic Foam Syntac® 351 is a castable syntactic composite material of epoxy resin and high performance hollow glass microspheres designed specifically for molding thermoforming plugs and other associated tooli.. |