Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Modulus | 2.304 GPa | 334.2 ksi | ASTM D695 |
Daelim H&L Plavis-G15 DF 15% Graphite Filled Aromatic Polyimide Bearing Direct Formed. Plavis-G-15: Graphite 15 wt% filled, Self lubricating grade for wear and friction applications.General Plavis information for all grades:PLAVIS polyimide has nitrogen bonded to 3 ca.. |