Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Modulus | 2.30 GPa | 334 ksi | ASTM D695 |
Saint-Gobain Meldin® 7021 Isostatically Molded Graphite Filled Polyimide Melidin® 7021 is a self-lubricating thermosetting polyimide that contains 15% graphite filler. Melidin® 7021 has a low coefficient of friction and high heat resistance, and is best for high t.. |
|||
Compressive Modulus | 2.30 GPa | 334 ksi | ASTM D695 |
Saint-Gobain Meldin® 7211 Isostatically Molded Graphite and PTFE Filled Polyimide Finished parts and basic shapes made from 10% by weight PTFE and 15% by weight graphite filled polyimide material for applications requiring a very low coefficient of friction and self-lubricating p.. |
|||
Compressive Modulus | 2.30 GPa | 334 ksi | |
Abatron AboCast 8103-11 One Part Epoxy One component system. Information provided by Abatron, Inc.Processing: Shelf life 6-8 months at 25°C (77°F). Heat cured; Pot life 190 min. at 100°C (212°C). Peak exotherm 170°C (340°F). At.. |