Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Modulus | 138 GPa | 20000 ksi | |
Hexcel® HexPly® EH04 Epoxy Resin System, IM4 Fiber IM4 120 24" EH04 31%; Normalized to 55% fiber volume; 75°F, dryInformation provided by HexCel |
|||
Compressive Modulus | 137.9 GPa @Temperature 23.0 °C |
20000 ksi @Temperature 73.4 °F |
|
Hexcel® HexPly® F515 Epoxy Resin, T5A120 Carbon Tape Hexcel designation: TXX120-12"-F515; Fiber: IM6Information provided by HexCel |