Polymer Property : Compressive Modulus = 17500 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Modulus 121 GPa
17500 ksi
Hexcel® HexPly® EH04 Epoxy Resin System, Fortafil 510 Fiber
F510 150 24" EH04 38%; Normalized to 55% fiber volume; 75°F, dryInformation provided by HexCel
Compressive Modulus 121 GPa

@Temperature 23.0 °C
17500 ksi

@Temperature 73.4 °F
Hexcel® HexPly® F515 Epoxy Resin, TSR9120 Carbon Tape
Fiber: Toray® T700SInformation provided by HexCel