Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Modulus | 11.0 GPa | 1600 ksi | |
Cytec Thornel® VCK Carbon Cloth Laminate with Mil R-9299 Resin Data provided by the manufacturer, Amoco Performance Products, Inc.Carbon and graphite cloths, consisting entirely of flexible filaments, are produced by pyrolysis of rayon cloth at high temperature.. |
|||
Compressive Modulus | 11.0 GPa | 1600 ksi | |
Cytec Thornel® VCL Carbon Cloth Laminate with Mil R-9299 Resin Data provided by the manufacturer, Amoco Performance Products, Inc.Carbon and graphite cloths, consisting entirely of flexible filaments, are produced by pyrolysis of rayon cloth at high temperature.. |