Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Modulus | 1.035 GPa | 150.1 ksi | Z direction; ASTM D638 |
Rogers Corporation RT/duroid® 6202 High Frequency Laminate Features:Low loss for excellent high frequency performanceTight dielectric constant and thickness controlExcellent electrical and mechanical propertiesExtremely low thermal coefficient of dielectric.. |
|||
Compressive Modulus | 1.035 GPa | 150.1 ksi | Z direction; ASTM D638 |
Rogers Corporation RT/duroid® 6202PR High Frequency Laminate Features:Low loss for excellent high frequency performanceTight dielectric constant and thickness controlExcellent electrical and mechanical propertiesExtremely low thermal coefficient of dielectric.. |