Polymer Property : Compressive Modulus = 0.0180 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Modulus 0.000124 GPa
0.0180 ksi
Force to Compress, Value given for 25% compression; ASTM D1667
Saint-Gobain Korel® K40-20 Medium Deflection Micro-cellular Polyurethane Foam
Description: The Korel® series micro-cellular polyurethane foams are offered in a broad range of properties, making them ideal for a variety of gasketing and energy absorption needs. Korel® mi..