Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Modulus | 4.14 - 7.93 GPa | 600 - 1150 ksi | Average value: 5.63 GPa Grade Count:3 |
Overview of materials for Polyamide-Imide, Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyamide-Imide, Glass Filled". Each property range of values reported is minimum and maximum values of .. |