Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Modulus | 36.0 - 119.3 GPa @Temperature -59.0 - 130 °C |
5220 - 17300 ksi @Temperature -74.2 - 266 °F |
Average value: 84.5 GPa Grade Count:11 |
Overview of materials for Epoxy/Carbon Fiber Composite This property data is a summary of similar materials in the MatWeb database for the category "Epoxy/Carbon Fiber Composite". Each property range of values reported is minimum and maximum values of a.. |