Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Modulus | 50.0 GPa @Temperature 23.0 °C |
7250 ksi @Temperature 73.4 °F |
prEN2580 Type B |
Hexcel® HexPly® M48 180°C/356°F Curing Epoxy Matrix, M48/42%/48370/1000 Fiber: HR 12K, 2x2 Twill, 370 g/m2Information provided by HexCel |
|||
Compressive Modulus | 50.0 GPa @Temperature 100 °C |
7250 ksi @Temperature 212 °F |
90º, Wet; DIN65380 |
Hexcel® HexPly® M12 135°C Curing Epoxy Matrix, 45% 46280 Fiber Information provided by HexCel |