Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Modulus | 4.82 GPa | 699 ksi | |
Henkel Hysol EA 9377 Paste Adhesive System Moldable plastic shim, excellent microcracking resistance under thermal cycling. High compressive strength.Application: Liquid Shim |