Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Modulus | 3.45 GPa | 500 ksi | Mixed 2:1; TM R050-38 |
Resinlab® EP1215 Clear Unfilled Epoxy Structural Adhesive Resinlab™ EP1215 Clear is a two part unfilled epoxy structural adhesive designed for bonding applications requiring high strength and good impact resistance. It cures completely at room temperature.. |
|||
Compressive Modulus | 3.45 GPa | 500 ksi | TM R050-38 |
Resinlab® EP1285HD-16 Highly Filled, Medium Viscosity Casting Resin Resinlab™ EP1285 (Formerly Lab Product W021901 series) is a highly filled, medium viscosity black casting resin designed for applications requiring a high degree of thermal conductivity and a low C.. |
|||
Compressive Modulus | 3.45 GPa | 500 ksi | ASTM D695 |
Quadrant EPP Ketron® 1000 LSG PEEK, Extruded Unfilled Polyetherether Ketone (ASTM Product Datasheet) |
|||
Compressive Modulus | 3.45 GPa | 500 ksi | ASTM D695 |
Quadrant EPP Ketron® 1000 PEEK, Extruded Unfilled Polyetherether Ketone (ASTM Product Data Sheet) |
|||
Compressive Modulus | 3.45 GPa | 500 ksi | ASTM D695 |
Quadrant EPP Ketron® CM GF30 Compression Molded, 30% Glass Reinforces Polyethererther Ketone(ASTM Product Data Sheet) |
|||
Compressive Modulus | 3.45 GPa @Temperature 22.8 °C |
500 ksi @Temperature 73.0 °F |
ASTM D695 |
Quadrant EPP Ketron® HPV PEEK High Pressure Velocity Polyetherether Ketone (ASTM Product Data Sheet) This bearing grade of extruded Ketron PEEK offers the lowest coefficient of friction and best machinability of all Ketron grades. It is ideal for low wear, high PV parts that require chemical resis.. |
|||
Compressive Modulus | 3.45 GPa | 500 ksi | Stabilized, typ, preliminary |
Hexcel® HexWeb® CR III 1/16-5056-.001 Corrosion Resistant Specification Grade Aluminum Honeycomb Grade is designated as "Cell Size-Alloy-Foil Gauge."5052 and 5056 expanded aerospace grade aluminum honeycomb materials are available in a wide selection of cell sizes and foil gauges. The HexWeb CR.. |
|||
Compressive Modulus | 3.45 GPa | 500 ksi | ASTM D695 |
Ensinger Tecapeek® XP-103 Compression Molded PEEK Compound, 15% Carbon Fiber Ensinger Special Polymers offers over twenty different VICTREX® PEEK blends to choose from and has the capability to blend custom compounds for specific applications. Compression molding results in.. |
|||
Compressive Modulus | 3.45 GPa | 500 ksi | ASTM D695 |
Ensinger Tecapeek® XP-99 Compression Molded PEEK Compound, Bearing Grade Material with 7% Graphite, 8% PTFE, and 15% Carbon Fiber Ensinger Special Polymers offers over twenty different VICTREX® PEEK blends to choose from and has the capability to blend custom compounds for specific applications. Compression molding results in.. |
|||
Compressive Modulus | 3.45 GPa | 500 ksi | ASTM D695 |
CIP Composites 100 Series Laminated Polymer Bearing Material The 100 series consists of polyester fabric and one of several solid lubricants (optional) in a resin matrix. Non-metallic, high load, high impact and self lubricating laminated material. Laminated.. |
|||
Compressive Modulus | 3.45 - 4.00 GPa | 500 - 580 ksi | Average value: 3.72 GPa Grade Count:6 |
Overview of materials for Polyetheretherketone, Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyetheretherketone, Glass Fiber Filled". Each property range of values reported is minimum and maximum.. |
|||
Compressive Modulus | 3.45 - 5.17 GPa | 500 - 750 ksi | Average value: 4.41 GPa Grade Count:5 |
Overview of materials for Epoxy, Cast, Metal Filled This property data is a summary of similar materials in the MatWeb database for the category "Epoxy, Cast, Aluminum Filled". Each property range of values reported is minimum and maximum values of a.. |
|||
Compressive Modulus | 3.45 GPa @Temperature 22.8 °C |
500 ksi @Temperature 73.0 °F |
ASTM D695 |
Quadrant EPP Duratron® U2200 PEI Extruded 20% Glass Reinforced Polyetherimide |
|||
Compressive Modulus | 3.45 GPa | 500 ksi | ASTM D695 |
Quantum PEEK Information provided by Quantum Advanced Engineering Plastics |
|||
Compressive Modulus | 3.45 GPa | 500 ksi | TM R050-38 |
Resinlab® EP1190 Flame Retardant Epoxy Casting Resin Resinlab™ EP1190 is a medium viscosity, flame retardant epoxy casting resin system. It is recognized under the Component Recognition Program of Underwriters Laboratories Inc., (File# E186034, Proje.. |