Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Modulus | 2.365 GPa | 343.0 ksi | |
Trelleborg Emerson & Cuming Eccolite® Composite Materials Ultra Syntactic Foam Eccolite Ultra syntactic foam plug assist materials a new engineered thermoplastic compound incorporating Eccospheres, glass microspheres. It is one of the toughest materials designed for the therm.. |