Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Modulus | 1.99 GPa | 288 ksi | ASTM D695 |
Westlake Plastics Radel® R 4400 Polyphenylsulfone For Medical Applications Medical grade Radel R4400 resin offers exceptional hydrolytic stability, toughness, heat deflection temperature and resistance to stress cracking. This polymer also has excellent thermal stability,.. |