Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Modulus | 1.86 GPa | 270 ksi | ASTM D695 |
Quadrant EPP Acetron® MD Metal-detectable Copolymer Acetal (ASTM Product Data Sheet) Low moisture absorption High strength, stiffness Easy to machine No centerline porosity in Acetron® GP Many formulation options: Copolymer, Homopolymer, PTFE filled, and Internally lubricated/enha.. |
|||
Compressive Modulus | 1.86 GPa | 270 ksi | Stabilized, typ |
Hexcel® HexWeb® CR III 3/16-5056-.002 Corrosion Resistant Specification Grade Aluminum Honeycomb Grade is designated as "Cell Size-Alloy-Foil Gauge."5052 and 5056 expanded aerospace grade aluminum honeycomb materials are available in a wide selection of cell sizes and foil gauges. The HexWeb CR.. |
|||
Compressive Modulus | 1.86 GPa | 270 ksi | Stabilized, typ |
Hexcel® HexWeb® CR-PAA™ 3/16-5056-0.002 Phosphoric Acid Anodized Aluminum Honeycomb Grade is designated as "Cell Size-Alloy-Foil Gauge." The life cycle of aluminum honeycomb sandwich structures in a given application can be directly related to the quality of the bond between the fa.. |
|||
Compressive Modulus | 1.86 GPa | 270 ksi | |
Abatron AboWeld/AboCure 7812-2 Thixotropic Epoxy AboWeld/AboCure 7812-2 is an underwater and cold-weather structural and dielectric adhesive paste. It is a 2-component thixotropic epoxy compound for dry, wet, and cold applications. It has many spe.. |
|||
Compressive Modulus | 1.86 GPa | 270 ksi | |
Abatron AboCast 50-16/AboCure 50-17 Epoxy Information provided by Abatron, Inc.Processing: Shelf life: 12+ months (unmixed). 100/28 ratio. Pot life: 500 g, 29 min. at 70°C (160°F). Exothermic Peak 242°C (468°F). Cures in 1-2 hrs at .. |