Compressive Modulus 0.883 GPa
128 ksi
ASTM D695
Saint-Gobain Fluoroloy® A30 High Performance PTFE/Glass Seal Material
Excellent heat, wear, and chemical resistance; Good cryogenic properties; Can be abrasive running against soft metals at high surface speed; Excellent material for back-up rings Information ..