Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Modulus | 0.0700 GPa | 10.2 ksi | average; perpendicular to plane; DIN 53421 |
3A Composites Core Materials AIREX® T92.80 Easy Processing Structural Foam AIREX® T92 is a closed-cell, thermoplastic and recyclable polymer foam with good mechanical properties and price / performance ratio. It has a good resistance to fatigue, is chemically stable, UV r.. |
|||
Compressive Modulus | 0.0700 GPa | 10.2 ksi | average; perpendicular to plane; DIN 53421 |
3A Composites Core Materials AIREX® C71.55 Elevated Temperature Structural Foam AIREX® C71 is a closed cell, crosslinked polymer foam especially formulated to maintain its stability also at higher processing or service temperatures. It combines excellent stiffness and strength.. |