Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Modulus | 0.0300 GPa | 4.35 ksi | average; perpendicular to plane; DIN 53421 |
3A Composites Core Materials AIREX® R63.50 Damage Tolerant Foam AIREX® R63 is a closed-cell, linear, thermoplastic polymer foam with high damage tolerance. This one of a kind formula combines very high elongation and excellent bond strength. AIREX® R63 is cold.. |
|||
Compressive Modulus | 0.0300 GPa | 4.35 ksi | Elasticity; Short term E; DIN EN 826 |
BASF Styrodur® 4000 CS Extruded Rigid Polystyrene Foam (Europe) Description: Styrodur C is the green extruded rigid polystyrene foam (XPS) from BASF. As a thermal insulation, it makes a significant contribution to climate protection by reducing CO2 emissions. Th.. |