Polymer Property : Compressive Modulus = 0.0158 GPa
Polymer Property :
Compressive Modulus =
0.0158 GPa
Product List
Mechanical Properties
Tips:
30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties
Metric
English
Comments
Compressive Modulus
0.0158
GPa
2.29
ksi
0.1; ASTM D695
Toyobo PELPRENE™ S2002FB Polyester TPE, Flame Resistant
Features: Polyester TPE, Flame ResistantInformation provided by Toyobo.