Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Modulus | 0.0000276 GPa | 0.00400 ksi | Force to Compress, Value given for 25% compression; ASTM D1667 |
Saint-Gobain Korel® K20 Very Soft Micro-cellular Polyurethane Foam Description: The Korel® series micro-cellular polyurethane foams are offered in a broad range of properties, making them ideal for a variety of gasketing and energy absorption needs. Korel® mi.. |
|||
Compressive Modulus | 0.0000276 - 1.15 GPa | 0.00400 - 167 ksi | Average value: 0.0996 GPa Grade Count:34 |
Overview of materials for Thermoset Polyurethane Foam, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Thermoset Polyurethane Foam, Unreinforced". Each property range of values reported is minimum and maximu.. |