Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Yield Strength | 184 - 474 MPa | 26700 - 68700 psi | Average value: 279 MPa Grade Count:4 |
Overview of materials for Thermoplastic Polyimide, Carbon Fiber This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Polyimide, Carbon Fiber". Each property range of values reported is minimum and maximum va.. |