Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Yield Strength | 110 - 380 MPa | 16000 - 55100 psi | Average value: 237 MPa Grade Count:63 |
Overview of materials for Phenolic, Novolac, Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Novolac, Glass Filled". Each property range of values reported is minimum and maximum values o.. |