Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Yield Strength | 28.0 - 241 MPa | 4060 - 35000 psi | Average value: 145 MPa Grade Count:18 |
Overview of materials for Nylon 66, 30% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 30% Glass Fiber Filled". Specific grades with glass content between 25% and 34% are included. .. |
|||
Compressive Yield Strength | 100 - 241 MPa | 14500 - 35000 psi | Average value: 133 MPa Grade Count:25 |
Overview of materials for Polyethersulfone (PES) This property data is a summary of similar materials in the MatWeb database for the category "Polyethersulfone". Each property range of values reported is minimum and maximum values of appropriate M.. |
|||
Compressive Yield Strength | 148 - 241 MPa | 21500 - 35000 psi | Average value: 193 MPa Grade Count:5 |
Overview of materials for Polyethylene Terephthalate (PET), 30% Glass Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), 30% Glass Reinforced". Specific grades with glass content between 25% .. |