Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Yield Strength | 152 - 189 MPa | 22000 - 27400 psi | Average value: 172 MPa Grade Count:4 |
Overview of materials for Polyphthalamide (PPA), Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, Mineral Filled". Each property range of values reported is minimum and maximum values o.. |