Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Yield Strength | 110 - 138 MPa | 16000 - 20000 psi | Average value: 120 MPa Grade Count:7 |
Overview of materials for Polycarbonate, 30% Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, 30% Glass Filled". Specific grades with glass content between 25% and 34% are included. E.. |
|||
Compressive Yield Strength | 26.0 - 138 MPa | 3770 - 20000 psi | Average value: 87.0 MPa Grade Count:11 |
Overview of materials for Nylon 6, Glass Fiber/Solid Lube Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Glass Fiber/Solid Lube Filled". Each property range of values reported is minimum and maximum v.. |
|||
Compressive Yield Strength | 124 - 138 MPa | 18000 - 20000 psi | Average value: 131 MPa Grade Count:8 |
Overview of materials for Polyethersulfone (PES), 20% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyethersulfone (PES), 20% Glass Fiber Filled". Each property range of values reported is minimum and m.. |
|||
Compressive Yield Strength | 49.6 - 138 MPa | 7200 - 20000 psi | Average value: 73.8 MPa Grade Count:8 |
Overview of materials for Polybutylene Terephthalate (PBT), Glass Bead Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Glass Bead Filled". Each property range of values reported is minimum .. |