Polymer Property : Compressive Yield Strength = 18000 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Yield Strength 117 - 124 MPa
17000 - 18000 psi
Average value: 122 MPa Grade Count:6
Overview of materials for Polybutylene Terephthalate (PBT), 30% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), 30% Glass Fiber Filled". Specific grades with glass content between 25..
Compressive Yield Strength 96.5 - 124 MPa
14000 - 18000 psi
Average value: 114 MPa Grade Count:8
Overview of materials for Polycarbonate, 20% Glass Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, 20% Glass Filled". Specific grades with glass content between 15% and 24% are included. E..
Compressive Yield Strength 110 - 124 MPa
16000 - 18000 psi
Average value: 114 MPa Grade Count:4
Overview of materials for Acrylic, Cast
This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, Cast". Each property range of values reported is minimum and maximum values of appropriate MatW..
Compressive Yield Strength 117 - 124 MPa
17000 - 18000 psi
Average value: 119 MPa Grade Count:3
Overview of materials for Acrylic, Optical Sheet
This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, Optical Sheet". Each property range of values reported is minimum and maximum values of appropr..
Compressive Yield Strength 53.8 - 124 MPa
7800 - 18000 psi
Average value: 77.7 MPa Grade Count:3
Overview of materials for Polybutylene Terephthalate (PBT), Glass + Mineral Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Glass + Mineral Filled". Each property range of values reported is min..