Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Yield Strength | 0.0650 - 0.0900 MPa | 9.43 - 13.1 psi | 25% Compression |
BIW ASTM Class 2D3 Silicone Foam Products are a closed cell foam and there fore good for use in damp or liquid applications. A variety of physical properties and foam qualities are available by adjusting the processing parameters... |
|||
Compressive Yield Strength | 0.0480 - 0.0900 MPa | 6.96 - 13.1 psi | at 25% deflection; 0.2"/min strain rate |
Rogers Corporation Poron® 4701-40-20 Cellular Urethane Foam Standard color is black (04); others are available. Passes flammability tests UL HBF (File E20305), MVSS 302, and CSA Component Acceptance HBF (File 188149). Passes fogging test SAE-J 1736 for 3 h.. |