Mechanical Properties Metric English Comments
Compressive Yield Strength 76.4919 - 76.5318 MPa

@Temperature 149 - 150 °C
11094.2 - 11100.0 psi

@Temperature 300 - 302 °F
Average value: 76.5 MPa Grade Count:2
Overview of materials for Thermoplastic Polyimide, Unfilled