Mechanical Properties Metric English Comments
Compressive Yield Strength 5.17 MPa
750 psi
TM R050-38
Resinlab® EP1121 Clear Electronic Grade Epoxy Encapsulant
Resinlab™ EP1121 Clear is a two part unfilled electronic grade epoxy encapsulant designed for small to medium sized castings. It cures completely at room temperature to a tough, flexible polymer. I..
Compressive Yield Strength >= 5.17 MPa
>= 750 psi
Stabilized, min
Hexcel® HexWeb® CR III 3/8-5052-.005 Corrosion Resistant Specification Grade Aluminum Honeycomb
Grade is designated as "Cell Size-Alloy-Foil Gauge."5052 and 5056 expanded aerospace grade aluminum honeycomb materials are available in a wide selection of cell sizes and foil gauges. The HexWeb CR..
Compressive Yield Strength >= 5.17 MPa
>= 750 psi
Stabilized, min
Hexcel® HexWeb® CR-PAA™ 3/8-5052-0.005 Phosphoric Acid Anodized Aluminum Honeycomb
Grade is designated as "Cell Size-Alloy-Foil Gauge." The life cycle of aluminum honeycomb sandwich structures in a given application can be directly related to the quality of the bond between the fa..
Compressive Yield Strength >= 5.17 MPa
>= 750 psi
Stabilized, min
Hexcel® HexWeb® HRP - 3/16 - 5.5 Fiberglass/Phenolic Honeycomb
Designation: Material-Cell Size (inches)-DensityHexWeb HRP is a glass fabric reinforced honeycomb in which a heat-resistant phenolic resin is used both for initial and final impregnations. This prod..
Compressive Yield Strength 5.17 MPa
750 psi
TM R050-38
Resinlab® EP1121 Black Electronic Grade Epoxy Encapsulant
Resinlab™ EP1121 Black is a two part unfilled electronic grade epoxy encapsulant designed for small to medium sized castings. It cures completely at room temperature to a tough, flexible polymer. I..
Compressive Yield Strength 5.17 MPa
750 psi
TM R050-38
Resinlab® EP1240RC Flame Retardant Epoxy Casting Resin
Resinlab™ EP1240RC is a medium viscosity, flame retardant epoxy casting resin system. It is recognized under the Component Recognition Program of Underwriters Laboratories Inc., (File# E186034, Pro..
Compressive Yield Strength 5.17 MPa
750 psi
Max load under tribological use
Saint-Gobain Rulon® J Grade Bearing/Seal PTFE
Description: Rulon® is the Saint-Gobain trade name for their family of proprietary PTFE compounds. This family of materials offers the combination of high compressive strength, low coefficient of f..