Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Yield Strength | 48.0 MPa | 6960 psi | |
Sawbones Solid Rigid Polyurethane Foam 50 pcf Density Solid Rigid Polyurethane FoamPrimary UseSolid rigid polyurethane foam is primarily used as an alternative test medium for human cancellous bone. These products are not intended to replicate the mech.. |
|||
Compressive Yield Strength | 48.0 MPa | 6960 psi | at 2.7% consolidation parallel to thickness |
Zircar Refractory Composites RSLE-501 CYLINDERS Refractory Sheet ZIRCAR Refractory Sheet Type RSLE-501 is a low expansion high strength reinforced silica matrix composites in a cylindrical form. This material was designed for use as a high strength, durable insul.. |
|||
Compressive Yield Strength | 48.0 MPa | 6960 psi | at 2.7% consolidation parallel to thickness |
Zircar Refractory Composites RSLE-57 Refractory Sheet ZIRCAR Refractory Sheet Type RSLE-57 is a low expansion high strength reinforced silica matrix composite . This material was designed for use as a high strength insulator in induction hot press appl.. |