Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Yield Strength | 435 MPa @Temperature 100 °C |
63100 psi @Temperature 212 °F |
90º, Wet; DIN65380 |
Hexcel® HexPly® M12 135°C Curing Epoxy Matrix, 45% 46280 Fiber Information provided by HexCel |