Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Yield Strength | 38.0 - 204 MPa | 5510 - 29600 psi | Average value: 107 MPa Grade Count:21 |
Overview of materials for Liquid Crystal Polymer (LCP), 30% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Liquid Crystal Polymer (LCP), 30% Glass Fiber Filled". Specific grades with glass content between 25% an.. |
|||
Compressive Yield Strength | 38.0 - 110 MPa | 5510 - 16000 psi | Average value: 71.0 MPa Grade Count:7 |
Overview of materials for Nylon 12 This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12". Each property range of values reported is minimum and maximum values of appropriate MatWeb en.. |