Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Yield Strength | 262 MPa | 38000 psi | ASTM D695 |
Sumitomo Bakelite North America 4064 Mineral Filled Electrical Encapsulation Grade Epoxy Rogers electrical encapsulation grade epoxy is recommended for capacitors, resistors, gold lead encapsulation, relays, coils and bobbins.Information provided by Sumitomo Bak North America, Inc. |
|||
Compressive Yield Strength | 262 MPa | 38000 psi | ASTM D695 |
Sumitomo Bakelite Durez® 23570 Phenolic, Injection Grade Durez 23570 Black Phenolic is a glass and mineral filled two-stage, special purpose molding material. It is designed for high strength, good dimensional stability, and electrical properties even aft.. |
|||
Compressive Yield Strength | 262 MPa @Temperature 23.0 °C |
38000 psi @Temperature 73.4 °F |
|
Hexcel® HexPly® 954-2A Curing Cyanate Resin, K1100 Fiber Information provided by HexCel |
|||
Compressive Yield Strength | 262 MPa | 38000 psi | transverse |
ATI Allegheny Ludlum Stainless Steel Type 301, annealed (UNS S30100) Allegheny Ludlum Type 301 is a high strength grade of steel available in six conditions or tempers, its resistance to atmosphere corrosion and its bright, attractive surface make it an excellent cho.. |
|||
Compressive Yield Strength | 262 MPa | 38000 psi | longitudinal |
ATI Allegheny Ludlum Stainless Steel Type 301, annealed (UNS S30100) Allegheny Ludlum Type 301 is a high strength grade of steel available in six conditions or tempers, its resistance to atmosphere corrosion and its bright, attractive surface make it an excellent cho.. |