Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Yield Strength | 221 MPa | 32100 psi | ASTM D695 |
Plenco 202 Black General Purpose Woodflour Filled Phenolic Molding Compound
(discontinued **) Plaslok 202 is a two-stage, woodflour-filled phenolic molding compound formulated to provide improved impact and fatigue strength, good dimensional stability and excellent molded finish for automoti.. |
|||
Compressive Yield Strength | 221 MPa | 32100 psi | ASTM D695 |
Plenco 501 Black Electrical Grade Mineral/Flock Filled Phenolic Molding Compound
(discontinued **) Plaslok 501 is a two-stage, mineral and flock-filled phenolic molding compound designed for use in heat resistant and electrical applications. It is designed for elevated temperature exposure for e.. |
|||
Compressive Yield Strength | 221 MPa | 32100 psi | ASTM D695 |
Plenco 504 Black (COM) Heat Resistant Mineral/Cellulose Filled Phenolic Molding Compound
(discontinued **)< Plaslok 504 is a two-stage, mineral and cellulose-filled phenolic molding compound having better impact and heat resistance than general purpose molding compounds. Since it also has good electrical.. |
|||
Compressive Yield Strength | 221 MPa | 32100 psi | ASTM D695 |
Plaslok 202 Black General Purpose Woodflour Filled Phenolic Molding Compound
(discontinued **) Plaslok Corporation was purchased by Plastics Engineering Company (maker of Plenco brand materials) in March 2000. The Plaslok name is no longer in use.Plaslok 202 is a two-stage, woodflour-filled .. |
|||
Compressive Yield Strength | 221 MPa | 32100 psi | ASTM D695 |
Plaslok 301 Black Impact Grade Woodflour/Flock Filled Phenolic Molding Compound
(discontinued **) Plaslok Corporation was purchased by Plastics Engineering Company (maker of Plenco brand materials) in March 2000. The Plaslok name is no longer in use.Plaslok 301 is a two-stage, woodflour and flo.. |
|||
Compressive Yield Strength | 221 MPa | 32100 psi | ASTM D695 |
Adell AW-17 Nylon 66, 35% Glass Reinforced; Superior Finish Data provided by Adell Plastics, Inc. |
|||
Compressive Yield Strength | 221 MPa | 32100 psi | ASTM D695 |
Adell AW-37 Nylon 66, 35% Glass Reinforced; Superior Finish Data provided by Adell Plastics, Inc. |
|||
Compressive Yield Strength | 221 MPa | 32100 psi | ASTM D695 |
Plenco 301 Black Impact Grade Woodflour/Flock Filled Phenolic Molding Compound
(discontinued **) Plaslok 301 is a two-stage, woodflour and flock-filled phenolic molding compound. It has broad molding latitude combined with good electrical properties and improved impact strength. It is particu.. |
|||
Compressive Yield Strength | 221 MPa | 32100 psi | ASTM D695 |
Plaslok 504 Black (COM) Heat Resistant Mineral/Cellulose Filled Phenolic Molding Compound
(discontinued **)&l Plaslok Corporation was purchased by Plastics Engineering Company (maker of Plenco brand materials) in March 2000. The Plaslok name is no longer in use.Plaslok 504 is a two-stage, mineral and cellu.. |
|||
Compressive Yield Strength | 221 MPa | 32100 psi | ASTM D695 |
Plaslok 501 Black Electrical Grade Mineral/Flock Filled Phenolic Molding Compound
(discontinued **) Plaslok Corporation was purchased by Plastics Engineering Company (maker of Plenco brand materials) in March 2000. The Plaslok name is no longer in use.Plaslok 501 is a two-stage, mineral and flock.. |