Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Yield Strength | 187 MPa | 27100 psi | ASTM D695 |
Sumitomo Bakelite North America 52-40-40-P Long-Glass Reinforced Diallyl Phthalate Ortho Resin Isomer (DAP). Used for critical, high-performance military and commercial electrical components where long-term reliability is demanded.Meets the requirements of ASTM D5948 Type GDI-30F.. |
|||
Compressive Yield Strength | 187 MPa | 27100 psi | |
Phenolic 46%, Carbon fabric 54% Phenolic - Monsanto "SC 1008". Carbon fabric - "VCA" |